Influence of the Amount of Master Alloy on the Properties of Austenitic Stainless Steel AISI 316L Powder Sintered in Hydrogen
Typ dokumentu
articlePeer-reviewed
publishedVersion
Autor
Skaloń , Mateusz
Kazior , Jan
Práva
Creative Commons Attribution 4.0 International Licensehttp://creativecommons.org/licenses/by/4.0/
openAccess
Metadata
Zobrazit celý záznamAbstrakt
AISI 316L austenitic stainless steel powder was modified with four different amounts of boron (0.1; 0.2; 0.3; 0.4 of wt. %) in the form of MasterAlloy micro-powder, and was sintered in a pure dry hydrogen atmosphere in order to obtain high density sintered samples characterized by a thickened non-porous surface layer. We investigated the influence of the amount of boron on: density, hardness, grain microhardness, porosity, microstructure and surface quality. The study revealed that it is possible by a conventional compacting and sintering process to obtain near full-density sintered samples with a non-porous superficial layer without boride precipitations.
Kolekce
K tomuto záznamu jsou přiřazeny následující licenční soubory:
Kromě případů, kde je uvedeno jinak, licence tohoto záznamu je Creative Commons Attribution 4.0 International License